What's new
British Ordnance Collectors Network

This is a sample guest message. Register a free account today to become a member! Once signed in, you'll be able to participate on this site by adding your own topics and posts, as well as connect with other members through your own private inbox!

WW2 French 47mm

Tuney

Well-Known Member
Three relic French 47mm tungsten tipped shells from the SA anti tank gun used by the Lorraine 37LCC tank waiting to go into electrolysis to remove all the rust. Missing there ballistic caps. Thank you Kie
 

Attachments

  • IMG_0247.jpeg
    IMG_0247.jpeg
    2 MB · Views: 49
Here is my 47mm capped projectile that is 145mm long.
There are 5 crimps holding the cap. Not sure if all are original or marks from somebody trying to unscrew the cap?
 

Attachments

  • French 47mm a.jpeg
    French 47mm a.jpeg
    502.5 KB · Views: 45
  • French 47mm b.jpeg
    French 47mm b.jpeg
    648.8 KB · Views: 44
Here is my 47mm capped projectile that is 145mm long.
There are 5 crimps holding the cap. Not sure if all are original or marks from somebody trying to unscrew the cap?
Hello Ron3350,
Not the same ; your shell is a M35 with penetration cap, others are M36 (Tuney : no tungsten) missing light magnesium ballistic caps (screwed).
It's difficult to find these caps in good condition because of the light alloy used. Shots and caps were stored separatly (a story said that gunners could fire shots without caps).
 
Last edited:
Hello Ron3350,
Not the same ; your shell is a M35 with penetration cap, others are M36 (Tuney : no tungsten) missing light magnesium ballistic caps (screwed).
It's difficult to find these caps in good condition because of the light alloy used. Shots and caps were stored separatly (a story said that gunners could fire shots without caps).
 

Attachments

  • IMG_0246.jpeg
    IMG_0246.jpeg
    106.9 KB · Views: 19
Also look at the tip of this corrosion everywhere apart from the tip
 

Attachments

  • IMG_0254.jpeg
    IMG_0254.jpeg
    2.1 MB · Views: 17
They are not tungsten tipped, but I assume the steel is an alloy with 3% tungsten, as they are really hard to cut and extremely hard to rasp, even after annealing.
 
Top